醋酸装置高速泵高速轴断裂原因分析及改进措施Reason Analysis and Improvement Measures of High Speed Pump Shaft Acetic Acid Device High-speed Fracture
苏本林,许炎,仝文浩
SU Ben-lin,XU yan,TONG Wen-hao
摘要(Abstract):
针对醋酸装置高速泵高速轴频繁发生断裂的现象,分别从高速轴断口宏观特性、轴的结构、转子部件动平衡精度以及材料耐腐蚀性能等方面进行原因分析,提出了结构上的改进和提高材料耐腐蚀性能的措施,经工业考核取得了良好的运行效果。
For high speed pump shaft acetic acid device high-speed frequent fracture of the phenomenon,respectively from the macroscopic characteristics 、the axis of the structure,dynamic balance of rotor accuracy and material corrosion resistant performance and so on,and some measures for corrosion resistance of the improvement of structure and improve the material was put forward,the industrial test achieved good results.
关键词(KeyWords):
高速轴;断裂;原因分析;改进措施
high speed shaft;fracture;cause analysis;improvement measures
基金项目(Foundation):
作者(Author):
苏本林,许炎,仝文浩
SU Ben-lin,XU yan,TONG Wen-hao
参考文献(References):
- [1]王丽鹃,张国福,宋天民,等.泵轴断裂原因分析[J].辽宁石油化工大学学报,2005,(9):43-46.
- [2]刘鸿文.材料力学[M].北京:高等教育出版社,1992.
- [3]许世文,黄满生,胡宗军,等.42Cr Mo合金钢疲劳试验研究[J].合肥工业大学学报,2008,(9):1506-1508.
- [4]成大先.机械设计手册[M].北京:化学工业出版社,1997.
- [5]杨帅,姜新阔,吴大转,等.离心泵通用自动化测试控制技术[J].排灌机械工程学报,2014,32(3):191-207.
- [6]吴为,朱明亮,轩福贞.微式样法测量25Cr2Ni Mo1V钢断裂韧度试验研究[J].压力容器,2015,35(3):15-19.
- [7]王勇,刘庆,刘东喜,等.不同叶片冲角离心泵内流诱导振动噪声研究[J].流体机械,2013,41(7):1-4,31.
- [8]赵国伟,盛建萍,杨军虎,等.离心泵叶轮主要几何参数与反作用度之间的关系研究[J].流体机械,2014,42(12):17-21.
- [9]丁遂栋.断裂力学[M].北京:机械工业出版社,1997.8
- [10]周伟,曲恒磊,赵永庆,等.热处理对TC4合金组织和性能的影响[J].热加工工艺,2005,(8),26-27.